SHIN KANA BUKATAR ALUMINUM EXTRUDED PROFILE na kwastan?
Za mu iya kuma samun daban-daban samuwa gami ga masana'antu na aluminum extrusionbayanan martaba, kamar 5052, 6061, 6063,7075 da ƙari. Kuma za mu iya isa sandblasting & anodized extruded karfe sassa, goga aluminum profiles, cnc aluminum gidaje, aluminum abubuwa tare da Laser haruffa da polishing aluminum kayayyakin.
Sunan: Madaidaicin aluminum extruded harsashi
Material: 6061 ko 6063 aluminum
Girman: 145*70.9*12.5mm
MOQ: 2K, Unlimited adadin samfurori
Tsari: aluminum extrusion + CNC + gogewa + tsaftacewa + cikakken dubawa + sandblasting anode + sassaka Laser
Manufa: ana amfani da shi azaman harsashi mai ƙarfi na taska na cajin wayar hannu
Mini-madaidaicin aluminum extrusion, yana nufin tsari na extrusion, ƙananan kauri na bangon bayanin martaba na aluminum tare da ƙayyadaddun buƙatu akan kayan aiki, kayan aiki, da fasaha shine 0.4mm, da extrusion tare da haƙuri. da ake bukata na ± 0.04mm ya zama daidai extrusion. Hakanan ana iya cewaƙaramin aluminum extrusion.
Gabaɗaya madaidaicin bayanan martaba na aluminum suna buƙatar juriya mai girma tsakanin ± 0.04 ~ 0.07mm
Mu -wani fasaha-suna da fiye da shekaru 10 na gwaninta a cikin samar da bayanan martaba daban-daban na aluminum. Abokan cinikinmu suna ci gaba da ƙalubalantar mu don samar da ƙarin sassan aluminum tare da siffofi na musamman da ƙayyadaddun juzu'i masu rikitarwa.
Idan kuna da buƙatu masu alaƙa, muna maraba da shawarar ku, zaku iya duba gidan yanar gizon mu don ƙarin koyo, ko ku kira mu don tuntuɓar kasuwanci ta 86+19926691505.
Cikakken Bayani
Suna: |
Power bank aluminum extrusion gidaje
|
Nau'in: |
Ƙananan extruded aluminum |
Girman: |
A girman da kuka nema |
Abu: |
AL6061/ AL 6063 |
Tsari: |
Aluminum extrued+CNC machining++ Sandblasting/Anodizing+Laser craving+Cikakken dubawa+Isarwa |
Aikace-aikace: |
Dace da ikon banki aluminum extrusion m harsashi |
Don kammala harsashi na e-cigare, wane irin matakai ake buƙata?
Mutuwa bude - aluminum extruding - gani yankan -CNC machining - polishing - nika - brushing - tsaftacewa - ingancin dubawa - marufi - kaya
Cikakkun bayanai
sawing
Sabuwar sigar e-cigare da aka fitar gabaɗaya tsawon mita 6 ce, sannan kuma harsashi e-cigare mai tsayi daban-daban ana sawn bisa ga girman buƙatun zane na abokin ciniki.
Injin CNC
Girman tsayin na'ura mai shinge gabaɗaya bai kai girman haƙurin zane ba. A wannan lokaci dole ne mu sanya kayan daya bayan daya akan na'urar CNC don sarrafa sirri (ciki har da tsayin daka da nau'i daban-daban - chamfering, hakowa, bude Windows, da dai sauransu, har ma da wasu samfurori dole ne a buga su da wani naushi don samun). siffar da kuke so.
Goge niƙa
Gabaɗaya yana nufin yin amfani da abubuwa masu ƙazanta (takardar yashi mai ɗauke da ɓangarorin tauri mai ƙarfi, da sauransu) don canza yanayin zahirin abubuwan saman ta hanyar sarrafa gogayya, babban maƙasudi shi ne samun takamaiman yanayin ƙasa.
A cewar samfurin surface fineness digiri na iya zabar zane dabaran, nailan dabaran, hemp dabaran, ruwa nika tsari. Bukatun saman samfur ba su da girma tare da dabaran zane, dabaran nailan, idan buƙatun suna da girma dole ne a yi amfani da dabaran hemp ko ma injin niƙa na ruwa.
Goge
Shin yin amfani da kyalle mai gogewa yana maimaituwa motsi, gogayya baya da gaba akan saman saman aikin aikin don haɓaka hanya, rubutun saman layin layi ne, na iya haɓaka ingancin farfajiyar kuma don rufe ƴan ƴan tarkacen saman.
Domin shawo kan lahani na surface taurin da kuma sa juriya na aluminum gami, fadada aikace-aikace kewayon da kuma mika rayuwar sabis, surface jiyya fasahar ya zama makawa mahada a cikin yin amfani da aluminum gami, da anodic hadawan abu da iskar shaka fasahar ne mafi yadu amfani. kuma mafi nasara daya a halin yanzu.
Aluminum anodized
Anodic hadawan abu da iskar shaka na aluminum tsari ne na electrolytic hadawan abu da iskar shaka tsari. A lokacin wannan tsari, ana canza fuskar aluminum da aluminum alloys a cikin fim din oxide, wanda ke da kariya, kayan ado da sauran kayan aiki.
Yashi mai fashewa
Yana da tsari na tsaftacewa da roughening surface na substrate ta hanyar tasiri mai sauri yashi kwarara, don haka da surface na workpiece iya samun wani mataki na tsabta da kuma daban-daban roughness.
Rini
Bayan conductive lura da aluminum guda za su bi Layer na oxide fim sa'an nan sanya a cikin launi Silinda za a iya canza launin.